Hei hi corrosion awmna hmun leh a awmna hmunah a innghat a ni. Surface rust tenau te hian hman dan pangngaiah nghawng a nei lo tlangpui a, mahse deep corrosion a awm emaw, zinc coating a chhe vek a, base material a corrode emaw a nih chuan product chu service atanga lakchhuah emaw thlak nghal emaw a ngai a ni.

 

A corrosion laka invenna mechanism chugalvanized steel wire rope hmanga siam a nia chunga zinc layer awm chu sacrificial anode anga thawkin inner steel wire te humhim turin a innghat a ni. Zinc layer chu zawi zawiin a ei zo emaw, a chhiat emaw chuan steel wire substrate chu a rust tan ang.

 

Corrosion Degree thliar hranna leh hman dan tehna

 

Corrosion Level a awm Hmuh theih dan (Visual Characteristics) te Hman theihna Thiltih tur rawtna
Light Corrosion (Lei chunglam Rust Spots) a awm thei. A chung lamah chuan reddish-brown rust spot theh darh a lang a, mahse zinc coating chu a tam zawk chu a la awm reng thung. Rust hian steel wire core chhungah a lut lo. ✔ Hman theih Anti-rust oil emaw grease emaw hmang la, routine inspection tih tam lehzual rawh.
A rilru a buai em em a, a rilru a hah em em bawk a. Rust patches chu a darh zel a. Steel wire chung lamah rust layer hmuh theih a lo awm a, mahse wire diameter-ah chuan tlahniam lian tham a awm lo va, wire chu a bendable reng a ni. ▲ Fimkhur takin hmang la, load rating chu downgrade rawh Chipchiar taka enfiah nghal tur (eg, diameter tehna, bend test). Load mamawh a tlem a, hman hun rei lote-a hman a nih chuan hnathawh dan uluk takin enfiah rawh; chutiang a nih loh chuan thlak a tha.
Hriselna nasa tak (Sectional Corrosion Loss) 1.1. Rust scale chu a flake off a, steel wire chung lamah pitting leh pits a awm ta a ni. Wire diameter chu hmuh theihin a tlahniam a, wire chhe pawh a lo lang thei bawk. ✗ Hman khap tlat a ni Hman dan kha titawp nghal la, steel wire rope zawng zawng chu thlak leh rawh.

 

Critical Warning Signs (Wire chhe lo pawhin Retired A ngai)

 

  • Wire chunglama pitting emaw grooves hmuh theih → Cross-sectional loss a awm a, chu chuan chakna nasa takin a tlahniam a ni.
  • Wire rope chu a khauh a, a hmin avangin a ben harsa → Internal corrosion nasa tak leh lubrication failed a nih thu a tarlang.
  • Rust scale chu lightly tapped a nih chuan a lianin a flake off → Zinc coating leh base metal pahnih hi a chhe vek tawh.
  • Hmun chhe tawha wire chhe tawh zawng zawng → Corrosion leh wire chhe tawhte inzawm chuan failure nasa takin a ti chak ang a, risk sang tak a ni.

 

Practical Hman dan tur rawtna

 

Dilna tur Scenario a ni Rust a lo awm hnuah Corrosion Tolerance a awm thei
Lifting & hoisting, passenger elevator, cable car te pawh a awm bawk Zero tolerance a ni: Red rust a awm chuan evaluate nghal tur a ni; moderate emaw higher emaw corrosion a awm chuan decommissioning nghal a ngai a ni.
In sakna tower crane, sakna hoist te Light corrosion hi pawm theih a ni a, mahse thla khatah vawi khat tal enfiah a ngai a ni.
A tlangpuiin industrial towing & conveying a ni Light corrosion hi pawm theih a ni a; moderate corrosion a awm chuan load operation tihtlem leh ruahman lawk thlak a ngai a ni.
Guy wire, lashing, fencing, non-load-bearing hmanna te a ni Moderate corrosion hi hun rei lote chhung atan hman theih a la ni a, mahse himna chu ngaih pawimawh hmasak a ngai thung.

 

 

Testing method chiang zawk emaw, hmanrua engtikah nge scrap tur tih hriat theihna tur tehfung table emaw i mamawh a nih chuan dilna angin kan pe thei ang.